Choose your hot-dip coated dual-phase steel here in grades HCT450X, HCT490X, HCT590X, HCT780X, HCT980X and HCT980XG.
The experts at our locations are happy to advise you. We look forward to hearing from you.
Short designation | VDA239-100* | Surface finish | Material number |
HCT450X | - | +Z, +ZF | 1.0937 |
HCT490X | CR290Y490T-DP | +Z, +ZF, +ZM | 1.0995 |
HCT590X | CR330Y590T-DP | +Z, +ZF, +ZM | 1.0996 |
HCT780X | CR440Y780T-DP | +Z, +ZF | 1.0943 |
HCT980X | CR590Y980T-DP | +Z, +ZF | 1.0944 |
HCT980XG | CR700Y980T-DP | +Z, +ZF | 1.0997 |
Short designation | Proof stress Rp0,2 MPa | Tensile strength Rm MPa min. | Elongation at fracture A801)2) % min. | Strain hardening exponent n10-UE min. | Bake hardening index BH2 min. |
HCT450X | 260-340 | 450 | 27 | 0,16 | 30 |
HCT490X | 290-380 | 490 | 24 | 0,15 | 30 |
HCT590X | 330-430 | 590 | 20 | 0,14 | 30 |
HCT780X | 440-550 | 780 | 14 | - | 30 |
HCT980X | 590-740 | 980 | 10 | - | 30 |
HCT980XG | 700-850 | 980 | 8 | - | 30 |
Percentage biy weight % max. | ||||||||||
Short designation | C | Si | Mn | P | S | Altotal (span) | Cr+Mo | Nb+Ti | V | B |
HCT450X | 0,14 | 0,75 | 2,00 | 0,080 | 0,015 | 0,015-1,0 | 1,00 | 0,15 | 0,20 | 0,005 |
HCT490X | 0,14 | 0,75 | 2,00 | 0,080 | 0,015 | 0,015-1,0 | 1,00 | 0,15 | 0,20 | 0,005 |
HCT590X | 0,15 | 0,75 | 2,50 | 0,040 | 0,015 | 0,015-1,5 | 1,40 | 0,15 | 0,20 | 0,005 |
HCT780X | 0,18 | 0,80 | 2,50 | 0,080 | 0,015 | 0,015-2,0 | 1,40 | 0,15 | 0,20 | 0,005 |
HCT980X | 0,20 | 1,00 | 2,90 | 0,080 | 0,015 | 0,015-2,0 | 1,40 | 0,15 | 0,20 | 0,005 |
HCT980XG | 0,23 | 1,00 | 2,90 | 0,080 | 0,015 | 0,015-2,0 | 1,40 | 0,15 | 0,20 | 0,005 |
1) Reduced minimum values of elongation at rupture apply to product thicknesses t < 0.60 mm (minus 2 units).
2) For ZF-coated, products the minimum values of elongation at fracture are reduced by 2 unites.
For ZF-coated in thicknesses t < 0.60 mm, the minimum elongation at rupture is reduced by 4 units.
* Comparative grade, therefore minor deviations from DIN EN values possible