S355JR | 1.0145
Grade S355JR has a minimum yield strength of 355 MPa. The impact energy at a room temperature of 20°C is at least 27 joules.
Non-alloy/general structural steel
S355JR | 1.0145: Properties according to DIN EN 10 025-2
Steel type
Short designation | VDA239-100 | Material number |
S355JR | - | 1.0145 |
S355JR | 1.0145: Mechanical properties, transverse 1)
Upper yield strength ReH MPa min. | Tensile strength Rm MPa | Elongation at fracture A80 % min. | Elongation at fracture A 5 % min. | |||||
e ≤ 16 mm | e < 3 mm | 3 mm ≤ e ≤ 16 mm | e ≤ 1 mm | 1 mm < e ≤ 1.5 mm | 1.5 mm < e ≤ 2 mm | 2 mm < e ≤ 2.5 mm | 2.5 mm < e < 3 mm | 3 mm ≤ e < 16 mm |
355 | 510–680 | 470–630 | 12 | 13 | 14 | 15 | 16 | 20 |
S355JR | 1.0145: Chemical composition (heat analysis)
Percentage by weight % max. | ||||||
C | Si | Mn | P | S | N | Cu |
0.24 | 0,55 | 1.60 | 0.035 | 0.035 | 0.012 | 0.55 |
Your product of choice: S355JR | 1.0145
1) As rolling widths ≥ 600 mm are primarily used, transverse values generally apply, refer to DIN EN 10 025-2.