Choose your hot-dip coated ferrite-bainite-phase steel in the grades HDT450F and HDT580F here.
The experts at our locations are happy to advise you. We look forward to hearing from you.
Short designation | VDA239-100* | Surface finish | Material number |
HDT450F | HR300Y450T-FB | +Z | 1.0961 |
HDT580F | HR440Y580T-FB | +Z | 1.0994 |
Short designation | Proof stress Rp0,2 MPa | Tensile strength Rm MPa min. | Elongation at fracture A801)2) % min. | Strain hardening exponent n10-UE min. |
HDT450F | 300-420 | 450 | 24 | - |
HDT580F | 460-620 | 580 | 15 | - |
Percentage by weight % max. | ||||||||||
Short designation | C | Si | Mn | P | S | Altotal (span) | Cr+Mo | Nb+Ti | V | B |
HDT450F | 0,18 | 0,50 | 2,00 | 0,050 | 0,010 | 0,015-2,0 | 1,00 | 0,15 | 0,15 | 0,005 |
HDT580F | 0,18 | 0,50 | 2,00 | 0,050 | 0,010 | 0,015-2,0 | 1,00 | 0,15 | 0,15 | 0,01 |
1) Reduced minimum values of elongation at rupture apply to product thicknesses t < 0.60 mm (minus 2 units).
2) For ZF-coated, products the minimum values of elongation at fracture are reduced by 2 unites.
For ZF-coated in thicknesses t < 0.60 mm, the minimum elongation at rupture is reduced by 4 units.
* Comparative grade, therefore minor deviations from DIN EN values possible